Laser machining of silicon with bursts of ultra-short laser pulses: Factors influencing the process efficiency and surface quality (Conference Presentation)

Neuenschwander, Beat; Remund, Stefan Marco; Kramer, Thorsten (2019). Laser machining of silicon with bursts of ultra-short laser pulses: Factors influencing the process efficiency and surface quality (Conference Presentation) In: Račiukaitis, Gediminas; Makimura, Tetsuya; Molpeceres, Carlos (eds.) Laser Applications in Microelectronic and Optoelectronic Manufacturing (LAMOM) XXIV (p. 2). SPIE 10.1117/12.2513297

[img]
Preview
Text (PDF Vortrag)
Präsentation_Neuenschwander_final.pdf

Download (5MB) | Preview

For silicon machined with 10 ps pulses at 1064nm it was found that the specific removal rate increases by a factor of about 2.5 when an 8-pulse burst is used instead of single pulses [1]. This increase in the specific removal rate directly scales with a higher surface roughness. For copper and a 3-pulse burst the absorptance of a machined surface increases to about 200% of the one obtained with single pulses [2]. This can serve as an explanation for the higher specific removal rate observed in this case [3]. Actual calorimetric measurements on silicon show that the fraction of the incoming energy which is converted to heat is almost independent on the number of pulses per burst (a behavior which was observed for copper too) and the absorptance depends on the number of pulses. However, as the observed variations in the absorptance are only in the order of a few % and do not monotonically increase with the number of pulses per burst the change in the absorptance cannot explain the increase in the specific removal rate for pulse bursts on silicon. Additional experiments including calorimetry with varying intra-burst time differences and pulse energies as well as experiments concerning reflectivity and transmission will help to understand this behavior of silicon. [1] B. Jaeggi, D.J. Förster, B. Neuenschwander, OSA Technical Digest, CLEO (2018), AM1M.3 [2] B. Jaeggi, D. J. Foerster, R. Weber, B. Neuenschwander, Adv. Opt. Techn. 7, 175 (2018) [3] B. Neuenschwander, B. Jaeggi, D.J. Foerster, Th. Kramer, S. Remund, to be published in Proc. of ICALEO (2018)

Item Type:

Conference or Workshop Item (Speech)

Division/Institute:

School of Engineering and Computer Science > Institute for Surface Applied Laser, Phototonics and Surface Technologies ALPS
School of Engineering and Computer Science

Name:

Neuenschwander, Beat0000-0001-9715-8557;
Remund, Stefan Marco;
Kramer, Thorsten;
Račiukaitis, Gediminas;
Makimura, Tetsuya and
Molpeceres, Carlos

Subjects:

Q Science > QC Physics
T Technology > TA Engineering (General). Civil engineering (General)

ISBN:

9781510624535

Publisher:

SPIE

Language:

English

Submitter:

Beat Neuenschwander

Date Deposited:

04 Dec 2019 07:20

Last Modified:

04 Nov 2021 21:46

Publisher DOI:

10.1117/12.2513297

Additional Information:

Copyright (2019) Society of Photo‑Optical Instrumentation Engineers (SPIE). One print or electronic copy may be made for personal use only. Systematic reproduction and distribution, duplication of any material in this publication for a fee or for commercial purposes, and modification of the contents of the publication are prohibited

ARBOR DOI:

10.24451/arbor.9235

URI:

https://arbor.bfh.ch/id/eprint/9235

Actions (login required)

View Item View Item
Provide Feedback